DESCRIPTION :
The butadiene-alpha-methyl styrene ( styrene ) rubber is
produced by emulsion copolymerization obutadiene and alpha-methyl
styrene ( styrene ) at low temperatures with an emulsifier being a
mixture of disproportioned rosin soaps and synthetic fatty acids. The
AO-6 (polyguard) is used as an antioxidant. |
APPLICATION :
The butadiene-alpha-methyl styrene ( styrene ) rubber
finds its use in engineering rubber goods manufacture and in footwear
industry. The butadiene-alpha-methyl styrene ( styrene ) rubber is
similar to those to SBR 1502 |
SPECIFICATIONS: |
PARAMETERS |
STANDARDS |
Mooney viscosity MB ( 100 ° C ) |
48 - 58 |
Viscosity lot spread |
±4 |
Conditional tensile strength,
Not less than |
6.5 Mpa ( 270 kgs/cm2 ) |
Elongation at rupture, not less than |
550% |
Rebound elasticity, not less than |
37% |
Loss of the mass on drying, not more than |
0.35% |
Fraction of total mass |
Ash, not more than |
0.8% |
Cu |
0.002% |
Fe |
0.008% |
AO-6 |
1.0-2.0% |
Organic acids |
5.0-7.2% |
Organic acids soaps, not more than |
0.30% |
Amount of the second bonded monomer -
alphamethylstyrene |
22.-25% |
Amount of the second bonded monomer -
styrene |
22-25% |
|
STORAGE, TRANSPORTATION :
The butadiene-alpha-methyl styrene (styrene) rubber is
produced in the form of 30 kg piles, wrapped in a polyethylene film and
packed in four-layer paper bags. If required the rubber can be
delivered in containers. |
|
Product Name: SBR 1712 |
DESCRIPTION :
The butadiene-alpha-methyl styrene ( styrene ) rubber is
produced by emulsion copolymerization of butadiene and alpha-methyl
styrene ( styrene ) at low temperatures with an emulsifier being a
mixture of soaps, rosin and synthetic fatty acids.BTC-150 and BC-1
mixture is used as an antioxidant. |
APPLICATION :
SKMS-30 ARKM-27 ( SKS – 30 ARKM – 27 ) rubber is
all-purpose. In general it is used in tire industry and in engineering
goods manufacture. The processing properties, synthetic rubber
technology, performance and quantity of ingredients of SKMS-30 ARKM-27 (
SKS-30 ARKM-27 ) are similar to those to SBR 1712. |
SPECIFICATIONS: |
PARAMETERS |
STANDARDS |
Mooney Viscosity , MB (100º C) |
47-57 |
Viscosity Spread |
±4 |
Conditional tensile strength, Not less than |
22MPa ( 225 kgs/cm² ) |
Elongation at rupture |
550-750% |
Rebound elasticity, not less than |
20% |
Fraction of total mass |
Ash, not more than |
0.6% |
Organic acids |
5.0-6.4% |
Oil PN-6 |
26.5-29.0% |
Amount of the second bonded monomer -
alphamethylstyrene |
21-24% |
Amount of the second bonded monomer -
styrene |
22-25% |
|
STORAGE, TRANSPORTATION :
SKMS-30 ARKM-27 ( SKS -30 ARKM-27 ) rubber is produced in
the form of 30 kg piles, wrapped in a polyethylene film and packed in
four-layer paper bags. If required the rubber can be delivered in the
containers. |
|
CLOSE |